Emission Factor

C53G - heat treatable steel - coil

Interested in licensing this data?

Request a quote

Emission factor summary

Emission intensity of C53G - heat treatable steel - coil. WNR/DIN is 1.1213. Retrieved from Sustamize v3.2.0. For further information refer to https://docs.sustamizer.com/assets/ilcd-docs/V3.2.0/materials/metals/6f9e5dfa-0a05-4edc-b2d6-7f165e1b6a12.xml.Data quality flag: Methodology - Data quality rating is either not evaluated or reported as poor according to the source.

PropertyValue
NameC53G - heat treatable steel - coil
SectorMaterials and Manufacturing
CategoryMetals
SourceSustamize
Source DatasetSustamize Materials Database - Metals - V3.2.0
Region
Unit Type
Year
2024
Year Released
2025
Emission Factor
  • CO2e
    kg/kg
Scopes3.1
LCA Activity
cradle_to_gate
Supported CO2e Calculation Method
AR6
Data Versioning
  • Status: Current

API Reference

Activity ID
metals-type_c53g_heat_treatable_steel-shape_coil
UUID
c3741396-3e9a-4d4f-aa8d-c38c8a7d4926