Emission Factor

SAE 1060 - unalloyed quality steel with average >= 0.55 % c or rm >= 700 mpa - coil

Interested in licensing this data?

Request a quote

Emission factor summary

Emission intensity of SAE 1060 - unalloyed quality steel with average >= 0.55 % c or rm >= 700 mpa - coil. WNR/DIN is 1.9601. Retrieved from Sustamize v3.2.0. For further information refer to https://docs.sustamizer.com/assets/ilcd-docs/V3.2.0/materials/metals/5df34f66-5c29-4747-bdb9-37c50e421126.xml.Data quality flag: Methodology - Data quality rating is either not evaluated or reported as poor according to the source.

PropertyValue
NameSAE 1060 - unalloyed quality steel with average >= 0.55 % c or rm >= 700 mpa - coil
SectorMaterials and Manufacturing
CategoryMetals
SourceSustamize
Source DatasetSustamize Materials Database - Metals - V3.2.0
Region
Unit Type
Year
2024
Year Released
2025
Emission Factor
  • CO2e
    kg/kg
Scopes3.1
LCA Activity
cradle_to_gate
Supported CO2e Calculation Method
AR6
Data Versioning
  • Status: Current

API Reference

Activity ID
metals-type_sae_1060_unalloyed_quality_steel_with_average_gte_0.55_percent_c_or_rm_gte_700_mpa-shape_coil
UUID
bf4c3509-5109-4422-9441-c79620e72b6e
Code Snippet
View API Docs